Material Notes:
Description: Provides Positive Seal in Log Home Joints: Norseal® Log Home Foam® V790 is a medium-density foam specifically developed for log home gasketing. Under a minimum of 25 percent compression, V790 provides an air, water and dust seal in all common log home joint designs. Compatible with all commonly used wood preservatives, Norseal® Log Home Foam® V790 maintains dimensional integrity. It will not cold flow, eliminating unsightly oozing, and its cellular foam substrate allows it to conform to curved and irregular surfaces.Stays Flexible for Easy Application: The low force to compress of Norseal® Log Home Foam® V790 permits easy assembly. It stays flexible at low temperatures for easy application and fast recovery. Formulated for good compression set properties, the foam provides a uniform (constant) seal during both initial construction and subsequent settling and shrinkage of seasoned logs.Excellent Adhesives Eases Assembly: A high-performance acrylic adhesive on one side speeds installation. Norseal® Log Home Foam® V790's excellent adhesive properties, combined with the low force to compress, permits rapid stacking, aligning and spiking of log tiers. An easy-release paper liner eliminates stretch during application and aids in the placements of the gasket. The rectangular tape profile adapts to all common joint designs.FEATURES/BENEFITS: Maintains dimensional integrity; Low force to compress permits easy assembly; Conforms to curved and irregular surfaces; Compatible with all commonly used wood preservatives; Stays flexible at low temperatures; Rectangular tape profile adapts to most joint designs; Provides excellent adhesion to wood.Typical applications include: Log homes, high-movement joints, low temperature sealing, lid seals of medical waste containers. All data based on a 0.25 inch test sample.(Available in thicnkesses from 1/4" to 1/2".) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.241 g/cc
0.00870 lb/in³
ASTM D1667
Water Absorption 8.0 %
8.0 %
% by volume; NTP-35
Mechanical Properties Metric English Comments
Hardness, Shore OO 20
20
ASTM D2240
Tensile Strength, Yield 0.221 MPa
32.0 psi
Norton Test Procedure 7
Elongation at Break 105 %
105 %
Norton Test Procedure 8
Compressive Strength 0.0124 MPa
1.80 psi
Force to Compress, 10% compression; Norton Test Procedure 10
0.0234 MPa
3.40 psi
Force to Compress, 25% compression; Norton Test Procedure 10
0.0434 MPa
6.30 psi
Force to Compress, 50% compression; Norton Test Procedure 10
0.103 MPa
14.9 psi
Force to Compress, 65% compression; Norton Test Procedure 10
0.257 MPa
37.3 psi
Force to Compress, 75% compression; Norton Test Procedure 10
Compression Set 2.0 %

@Temperature 37.8 °C
2.0 %

@Temperature 100 °F
Constant Deflection, Value given for 50% compression, after 6 days; Norton Test Procedure 37
3.0 %

@Temperature 37.8 °C
3.0 %

@Temperature 100 °F
Constant Deflection, Value given for 75% compression, 6 days; Norton Test Procedure 37
4.0 %

@Temperature 70.0 °C
4.0 %

@Temperature 158 °F
Constant Deflection, Value given for 50% compression, 6 days; Norton Test Procedure 37
5.0 %

@Temperature 70.0 °C
5.0 %

@Temperature 158 °F
Constant Deflection, Value given for 75% compression, 6 days; Norton Test Procedure 37
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Descriptive Properties Value Comments
Color Black