Material Notes:
Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tubing provides the most flexibility, highest temperature resistance and longest pump life available in a clear, plasticizer / oil free tubing. It is ideal for a broad range of applications including peristaltic pump applications, soap and detergent dispensing, water purification lines, food contact applications and chemical transfer. This uniquely engineered tubing will not embrittle or crack prematurely like other tubings that contain plasticizer or extender oils, benefiting the user with less downtime and tubing changes.Features/Benefits:Plasticizer and oil free -- does not contaminate fluidsSuperior flex life in peristaltic pumpsChemically resistant to a wide range of fluidsTemperature resistant from -108°F to 135°FClear for easy visual flow monitoringMeets FDA criteria for food contactIdeal for a broad range of demanding applications including peristaltic pump systems, soap and detergent dispensing, ink transfer, water purification lines, food and beverage, and chemical transfer.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ASTM D792-00
Water Absorption 0.040 %
0.040 %
24 hours at 23°C; ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
15 seconds; ASTM D2240-00
Tensile Strength, Yield 5.52 MPa
800 psi
ASTM D412-98
Elongation at Break 500 %
500 %
ASTM D412-98
100% Modulus 0.00165 GPa
0.240 ksi
ASTM D412-98
Tear Strength 24.5 kN/m
140 pli
Initial Tear Strength; ASTM D1004-94
Compression Set 40 %

@Temperature 70.0 °C
40 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-98 Method B
Tensile Set 110 %
110 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 57.2 °C
135 °F
Brittleness Temperature >= -77.8 °C
>= -108 °F
ASTM D746-98
-73.3 °C
-100 °F
Low Temperature Flexibility; ASTM D380-94
Electrical Properties Metric English Comments
Dielectric Strength 20.9 kV/mm
530 kV/in
ASTM D149-97
Descriptive Properties Value Comments
Color Clear