Saint-Gobain Tygon® R-3400 UV Resistant Tubing Formulation

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® R-3400 UV Resistant Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tygon® R-3400: Ideal for virtually any permanent or temporary chemical transfer application, Tygon® UV Resistant Tubing combines suppleness and flexibility with resistance to a wide range of chemicals. It shows exceptional resistance to strong acids and many alkalies. The flexibility of Tygon® UV Resistant Tubing makes it quick and easy to put into service, providing considerable savings on installation time and cost. Black in color, it is resistant to ultraviolet light, ozone and weathering, making it ideal for many outdoor applications. Standard sizes of Tygon® UV Resistant Tubing have sufficient wall thickness to block transmission of all UV light. Additionally, in-house testing indicates a UL 94V-O and UL 94HB flammability rating.Features/Benefits:Black in color; Protects light sensitive fluidsWide range of chemical resistanceOzone resistantExcellent burn resistanceLow compression set; Resists permanent deformationAvailable in clear formulation for fluid flow monitoringTypical applications include Acid and Caustic Transfer, Corrosive Diffusible Gases, Fertilizer and Pesticide Dispensing, Electrical Insulation Lines, Ink and Adhesive Dispensing, General MaintenanceInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792-91
Water Absorption 0.19 %
0.19 %
24 hours at 23°C; ASTM D570-95
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
15 seconds; ASTM D2240-97
Tensile Strength, Yield 15.5 MPa
2250 psi
ASTM D412-97
Elongation at Break 350 %
350 %
ASTM D412-97
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D412-97
Tear Strength 32.4 kN/m
185 pli
Initial Tear Strength; ASTM D1004-94
Compression Set 69 %

@Temperature 70.0 °C
69 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 66 %
66 %
ASTM D412-97
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -21.1 °C
-6.00 °F
ASTM D746-95
Electrical Properties Metric English Comments
Dielectric Strength 19.3 kV/mm
490 kV/in
ASTM D149-95
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: