Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® GR-4015A ABS, Glass Filled

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® GR-4015A ABS, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 72.6 MPa
10500 psi
5 mm/min; ASTM D638
Flexural Strength 98.1 MPa
14200 psi
2.8 mm/min; ASTM D790
Flexural Modulus 5.30 GPa
768 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.686 J/cm

@Thickness 3.17 mm
1.29 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 106 °C
223 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 - 1.65 mm
HB

@Thickness 0.0591 - 0.0650 in