Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® TX-0510T TRABS, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® TX-0510T TRABS, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 17 g/10 min

@Load 10.0 kg,
Temperature 220 °C
17 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 45.1 MPa
6540 psi
5 mm/min; ASTM D638
Flexural Strength 63.7 MPa
9240 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.27 J/cm

@Thickness 3.17 mm
2.39 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 - 3.00 mm
HB

@Thickness 0.0591 - 0.118 in
Optical Properties Metric English Comments
Haze 2.8 %

@Thickness 3.20 mm
2.8 %

@Thickness 0.126 in
ASTM D1003
Transmission, Visible 88 %

@Thickness 3.20 mm
88 %

@Thickness 0.126 in
ASTM D1003
Copyright © lookpolymers.com All Rights Reserved