Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schmelzer Industries Pearlveil 110-10 Fiberglass Veil

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Schmelzer Industries
Trade Name Pearlveil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmelzer Industries Pearlveil 110-10 Fiberglass Veil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmelzer Industries.
Mechanical Properties Metric English Comments
Hardness, Barcol 33
33
Tensile Strength, Ultimate 21.13 MPa
3065 psi
s.d. 1.72 MPa, test specimen 1.20 cm wide (s.d. 0.003 cm), 0.23 cm thick (s.d. 0.010 cm)
Elongation at Break 0.50 %
0.50 %
Elongation at max. load, 0.52%
Modulus of Elasticity 4.10 GPa
595 ksi
std. dev. 0.55 GPa
Flexural Strength 38.9 MPa
5640 psi
s.d. 2.1 MPa, specimen 2.50 cm wide (s.d. 0.008 cm), 0.24 cm thick (s.d.005 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Flexural Modulus 3.70 GPa
537 ksi
Tangent
Users viewing this material also viewed the following: