Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.58 g/cc
0.0932 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.60 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.78 µin/in-°F

@Temperature -22.0 - 158 °F
10.1 µm/m-°C

@Temperature 20.0 - 300 °C
5.61 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 480 °C
896 °F
Optical Properties Metric English Comments
Refractive Index 1.52

@Wavelength 587.6 nm
1.52

@Wavelength 587.6 nm
He
1.53

@Wavelength 404.7 nm
1.53

@Wavelength 404.7 nm
Hg
Transmission, Visible <= 1.0 %

@Wavelength 540 - 700 nm
<= 1.0 %

@Wavelength 540 - 700 nm
80 %

@Wavelength 390 - 400 nm
80 %

@Wavelength 390 - 400 nm
Internal transmittance of 87% from 390-400 nm
80 %

@Wavelength 400 - 410 nm
80 %

@Wavelength 400 - 410 nm
Internal transmittance of 87% from 400-410 nm
IR Transmittance 75 %

@Wavelength 2500 - 2600 nm
75 %

@Wavelength 2500 - 2600 nm
Internal transmittance of 82% at 2600 nm.
UV Transmittance <= 0.040 %

@Wavelength 200 - 310 nm
<= 0.040 %

@Wavelength 200 - 310 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0