Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.62 g/cc
0.0947 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.17 µin/in-°F

@Temperature -22.0 - 158 °F
8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 466 °C
871 °F
Optical Properties Metric English Comments
Refractive Index 1.53

@Wavelength 587.6 nm
1.53

@Wavelength 587.6 nm
He
1.54

@Wavelength 404.7 nm
1.54

@Wavelength 404.7 nm
Hg
Transmission, Visible 27 %

@Wavelength 690 nm
27 %

@Wavelength 690 nm
90 %

@Wavelength 450 - 530 nm
90 %

@Wavelength 450 - 530 nm
Internal transmittance of 98% from 450-530 nm
IR Transmittance 79 %

@Wavelength 2000 - 2100 nm
79 %

@Wavelength 2000 - 2100 nm
Internal transmittance of 86% from 2000-2100 nm.
UV Transmittance <= 0.60 %

@Wavelength 200 - 300 nm
<= 0.60 %

@Wavelength 200 - 300 nm
87 %

@Wavelength 390 nm
87 %

@Wavelength 390 nm
Internal transmittance of 95% at 390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 2
2
Alkali Class, AR 2
2
Stain Resistance Class, FR 0.0
0.0
Users viewing this material also viewed the following: