Material Notes:
Colloidally/ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.76 g/cc
0.0997 lb/in³
Thermal Properties Metric English Comments
CTE, linear 9.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.44 µin/in-°F

@Temperature -22.0 - 158 °F
10.7 µm/m-°C

@Temperature 20.0 - 300 °C
5.94 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 581 °C
1080 °F
Glass Temperature Coefficient 0.070
0.070
Optical Properties Metric English Comments
Refractive Index 1.54

@Wavelength 587.6 nm
1.54

@Wavelength 587.6 nm
He
Transmission, Visible <= 0.0010 %

@Wavelength 400 - 690 nm
<= 0.0010 %

@Wavelength 400 - 690 nm
0.40 %

@Wavelength 700 nm
0.40 %

@Wavelength 700 nm
Internal transmittance of 0.4% at 400 nm
0.40 %

@Wavelength 700 nm
0.40 %

@Wavelength 700 nm
IR Transmittance 88 %

@Wavelength 770 - 800 nm
88 %

@Wavelength 770 - 800 nm
Internal transmittance of 97% from 780-800 nm.
UV Transmittance <= 0.0010 %

@Wavelength 200 - 390 nm
<= 0.0010 %

@Wavelength 200 - 390 nm
Internal transmittance of less than 0.001% from 200-390 nm
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 4.4
4.4
Alkali Class, AR 1
1
Stain Resistance Class, FR 3
3