Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: Automotive exterior partsInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0667 g/cc
0.00241 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.82213 MPa
119.24 psi
ASTM D3575
Elongation at Break 6.2 %
6.2 %
ASTM D3575
Flexural Strength 0.80703 MPa
117.05 psi
ASTM D790
Flexural Modulus 0.031352 GPa
4.5472 ksi
ASTM D790
Compressive Strength 0.521 MPa

@Strain 25.0 %
75.5 psi

@Strain 25.0 %
ASTM D3575
0.6789 MPa

@Strain 50.0 %
98.47 psi

@Strain 50.0 %
ASTM D3575
1.2911 MPa

@Strain 75.0 %
187.26 psi

@Strain 75.0 %
ASTM D3575
Compression Set 43.7 %
43.7 %
ASTM D3575
Descriptive Properties Value Comments
Color White
Range of center value of pre-expanded particles 0.11-0.17 in
Users viewing this material also viewed the following: