Sekisui PIOCELAN LSP-20DB Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN LSP-20DB Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: Automotive exterior partsInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0500 g/cc
0.00181 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.80283 MPa
116.44 psi
ASTM D3575
Elongation at Break 7.7 %
7.7 %
ASTM D3575
Flexural Strength 0.5877 MPa
85.24 psi
ASTM D790
Flexural Modulus 0.024693 GPa
3.5814 ksi
ASTM D790
Compressive Strength 0.4058 MPa

@Strain 25.0 %
58.85 psi

@Strain 25.0 %
ASTM D3575
0.5239 MPa

@Strain 50.0 %
75.99 psi

@Strain 50.0 %
ASTM D3575
0.99822 MPa

@Strain 75.0 %
144.78 psi

@Strain 75.0 %
ASTM D3575
Compression Set 44.8 %
44.8 %
ASTM D3575
Descriptive Properties Value Comments
Color Black
Range of center value of pre-expanded particles 0.13-0.18 in