Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: General molded articlesInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.3253 MPa
47.18 psi
ASTM D3575
Elongation at Break 6.4 %
6.4 %
ASTM D3575
Flexural Strength 0.2357 MPa
34.19 psi
ASTM D790
Flexural Modulus 0.0097175 GPa
1.4094 ksi
ASTM D790
Compressive Strength 0.1662 MPa

@Strain 25.0 %
24.11 psi

@Strain 25.0 %
ASTM D3575
0.236 MPa

@Strain 50.0 %
34.2 psi

@Strain 50.0 %
ASTM D3575
0.4659 MPa

@Strain 75.0 %
67.58 psi

@Strain 75.0 %
ASTM D3575
Compression Set 41.2 %
41.2 %
ASTM D3575
Descriptive Properties Value Comments
Color White
Range of center value of pre-expanded particles 0.16-0.23 in