Material Notes:
Isocorâ„¢ HG20SC us a medium viscosity compounding grad PA-612 based nylon. This resin is specifically suited for applications requiring lower moisture regain and greater dimensional stability. Isocorâ„¢ HG20SC is used in applications requiring good electrical insulation properties. This resin can be processed with conventional techniques. Used for injection molding, automotive, lawn and garden, tubing, and films.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.039 g/cc
0.03754 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.4 MPa
4560 psi
ASTM D 638
Tensile Modulus 2.30 GPa
333 ksi
ASTM D 638
Izod Impact, Notched 0.366 J/cm
0.685 ft-lb/in
ASTM D 256
Gardner Impact 36.2 J

@Temperature 23.0 °C
26.7 ft-lb

@Temperature 73.4 °F
ASTM 5420
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ASTM D 3418-97
Processing Properties Metric English Comments
Moisture Content 0.17 %
0.17 %
ASTM D 570-95