Shakespeare Resistat® F9322 A061 Nylon 6 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Resistat® F9322 A061 Nylon 6 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resistat F9322, MERGE A061 is composed of a 22 denier nylon 6 monofilament, which has electrically conductive carbon suffused into the surface, combined with two ends of 70/30 polyester yarn. The components have been twisted together and heat set. The conductive filaments have a round cross section with a coating thickness of approximately 1 micron. The yarn color is gray. Resistat is used for carpeting, ESD garments, and industrial belting and brushes.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Fiber Count 189 dtex
170 denier
Mechanical Properties Metric English Comments
Elongation at Break 45 %
45 %
Tenacity 0.309 N/tex
3.50 g/denier
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Electrical Properties Metric English Comments
Electrical Resistivity 200000 ohm-cm
200000 ohm-cm