Material Notes:
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Calculated from diameter of 0.41 mm and product yield of 6760 m/kg.
Fiber Count 1480 dtex
1330 denier
Per Filament
Mechanical Properties Metric English Comments
Elongation at Break 30 %
30 %
Tenacity 0.441 N/tex
5.00 g/denier
7 kg breaking load
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
Shrinkage 5.00 %

@Temperature 175 °C,
Time 601 sec
5.00 %

@Temperature 347 °F,
Time 0.167 hour
Electrical Properties Metric English Comments
Electrical Resistivity 7000 ohm-cm
7000 ohm-cm
Average
<= 10000 ohm-cm
<= 10000 ohm-cm