Shakespeare WP-220 diameter 0.2 mm Weft Polyester Monofilament

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WP-220 diameter 0.2 mm Weft Polyester Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterModerate ModulusModerate shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 24 %
24 %
Elongation at Yield 5.0 %
5.0 %
at 3 g/D
Thermal Properties Metric English Comments
Shrinkage 12.0 %

@Temperature 175 °C
12.0 %

@Temperature 347 °F