Material Notes:
Outline of ACM ResinFor overcoming the shortcomings of plasticizers and CPE, we developed a new type impact modifier ACM which as a copolymer of HDPE and acrylic acid and our ACM not only has the basic feature of CPE, but has higher impact strength and lower glass temperature comparing with CPE, so its impact modification effect is more evident than CPE. Besides, ACM can effectively improve the weather-resistance of PVC products.ApplicationThe application method of ACM is the same as that of CPE. In processing, electric current and torque of extruders may have a slight decline and it may be eliminated through adjusting lubricant agent in the ingredients.Information Provided by Shandong Rike Chemical Co., Ltd.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 17.9 kJ/m²

@Temperature 0.000 °C
8.52 ft-lb/in²

@Temperature 32.0 °F
Phr = 0
19.8 kJ/m²

@Temperature 23.0 °C
9.42 ft-lb/in²

@Temperature 73.4 °F
Phr = 0
20.3 kJ/m²

@Temperature 0.000 °C
9.66 ft-lb/in²

@Temperature 32.0 °F
Phr = 5
22.3 kJ/m²

@Temperature 0.000 °C
10.6 ft-lb/in²

@Temperature 32.0 °F
Phr = 8
24.2 kJ/m²

@Temperature 23.0 °C
11.5 ft-lb/in²

@Temperature 73.4 °F
Phr = 5
25.3 kJ/m²

@Temperature 23.0 °C
12.0 ft-lb/in²

@Temperature 73.4 °F
Phr = 8
Descriptive Properties Value Comments
Balance Torque (N-m) 29.6
10 Phr
30
8 Phr
30.5
5 Phr
Fusion Temperature (°C) 178
5 Phr
178
8 Phr
178
10 Phr
Fusion Time (s) 203
10 Phr
212
8 Phr
241
5 Phr
Torque (N-m) 24.7-32.6
5 Phr
25.2-31.3
10 Phr
25.2-32.0
8 Phr