Material Notes:
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rotary Kiln, Heat Curing and Acid Proof Lining Industry Focuses: Steel, Sponge, Rolling Mills, Coke Oven, Ferrous Foundries, Non-Ferrous, Cement, Petro Chemical, Mineral Processing, Sugar / Paper Mills and Chemical PlantsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 2.30 g/cc
0.0831 lb/in³
Porosity 22 - 24 %
22 - 24 %
Mechanical Properties Metric English Comments
Compressive Strength 29.4 - 39.2 MPa
4270 - 5690 psi
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1450 °C
2640 °F
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
Fe2O3 2.5 %
2.5 %
Descriptive Properties Value Comments
PCE Orton 34
Permanent Linear Change -2.0 - 2.0%
1600°C