Sharadaa Ceramics HH 40 Normal Medium and High Heat and Super Duty Brick

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics HH 40 Normal Medium and High Heat and Super Duty Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rotary Kiln, Heat Curing and Acid Proof Lining Industry Focuses: Steel, Sponge, Rolling Mills, Coke Oven, Ferrous Foundries, Non-Ferrous, Cement, Petro Chemical, Mineral Processing, Sugar / Paper Mills and Chemical PlantsInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 2.10 g/cc
0.0759 lb/in³
Porosity 25 %
25 %
Mechanical Properties Metric English Comments
Compressive Strength 19.6 MPa
2840 psi
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1400 °C
2550 °F
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
Fe2O3 2.0 %
2.0 %
Descriptive Properties Value Comments
PCE Orton 32
Permanent Linear Change -1.0 - 1.0%
1400°C