Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Sharadaa Ceramics
Trade Name PHOSTCAST
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics PHOSTCAST 60 XL Phosphate Bonded Castables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and others. Made from quality material, our range is high on compressive strength, abrasion resistance and is capable to withstand extreme temperature.Note: We shall supply in two components namely in powder form and liquid form. The two components are to be mixed in the recommended proportion in a sand mixer and rammed by pneumatic tools or Hand ramming.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.40 g/cc
>= 0.0867 lb/in³
Grain Size <= 3000 µm
<= 3000 µm
Mechanical Properties Metric English Comments
Compressive Strength >= 19.6 MPa

@Temperature 110 °C
>= 2840 psi

@Temperature 230 °F
Cold Crushing
>= 49.0 MPa

@Temperature 1100 °C
>= 7110 psi

@Temperature 2010 °F
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1550 °C
2820 °F
Component Elements Properties Metric English Comments
Al2O3 >= 60 %
>= 60 %
Fe2O3 <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Permanent Linear Change 0.001
1400°C