Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Descriptive Properties Value Comments
Active (%) 100
Appearance Solid
INCI Acrylates/Stearyl Acrylate/Dimethicone Methacrylate Copolymer
Kind Wax Type
Nature of Silicone Rubber Core Silicone Acrylate
Softening Temperature 30
Viscosity Measurement Wax, cs