Shin-Etsu Silicones KE-5550U Low Temperature Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-5550U Low Temperature Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ShinEtsu KE5550 U is a nominal 50 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it also has excellent low temperature characteristics.Typical Applications: Electronic CD mounts.Motor and engine mounts.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength at Break 9.804 MPa
1422 psi
Elongation at Break 750 %
750 %
Tear Strength 21.9 kN/m
125 pli
Die B
Compression Set 7.0 %

@Temperature 180 °C,
Time 79200 sec
7.0 %

@Temperature 356 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH-50
Cure Type Post Cure