Shin-Etsu Silicones KF-6100 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KF-6100 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Viscosity Measurement 40000
40000
cs
Optical Properties Metric English Comments
Refractive Index 1.458
1.458
Descriptive Properties Value Comments
Active (%) 100
Appearance Liquid
Diluent (%) NA
HLB High
INCI Polyglyceryl-3 Disiloxane Dimethicone