Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SF11500U is a low Durometer and low modulus fluorosilicone with excellent processing ability.. Typical Applications: GasketsSealsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 15
15
Tensile Strength at Break 4.62 MPa
670 psi
Elongation at Break 875 %
875 %
100% Modulus 0.000207 GPa
0.0300 ksi
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Press Cure