Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones SV-17500U Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones SV-17500U Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SV17500U is one of a series of easy processing, silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product Features: This product can be blended with other ShinEtsu general purpose or no post cure bases for intermediate properties. The choice between these bases will depend on specific requirements..Typical Applications: Roll covers.Diaphragms.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
Tensile Strength at Break 9.93 MPa
1440 psi
Elongation at Break 330 %
330 %
100% Modulus 0.00293 GPa
0.425 ksi
Tear Strength 21.6 kN/m
123 pli
Die B
Compression Set 22 %

@Temperature 177 °C,
Time 79200 sec
22 %

@Temperature 351 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Press Cure
Users viewing this material also viewed the following: