Sibur BSK-1500 Styrene-Butadiene Rubber (SBR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur BSK-1500 Styrene-Butadiene Rubber (SBR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR-1502. For use in the tire industry for production of tire thread and other parts for tires, in rubber technical industry for production of a wide assortment of rubber technical articles, and in the shoe industry for production of white and colored rubber footwear.
Physical Properties Metric English Comments
Mooney Viscosity 45 - 57

@Temperature 100 °C
45 - 57

@Temperature 212 °F
ML 1-4
Ash <= 0.60 %
<= 0.60 %
Chemical Properties Metric English Comments
Styrene Content 21 - 24 %
21 - 24 %
Descriptive Properties Value Comments
Loss During Drying <0.5%
Mass Share of Santoflex-134 0.15-0.4%
Mass Share of VS-1 0.15-0.5%
Mass Share of VTS-150 1-1.4%
Spread Flow Batch Error <±8 %