Sibur DSSK-2545-M27 Oil-Filled Styrene-Butadiene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur DSSK-2545-M27 Oil-Filled Styrene-Butadiene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Buna VSL 5025-1. IN some compounding of rubber mixtures rubber can be used as replacement of butadiene styrene rubber and butadiene styrene rubber with preservation improvement of indexes of finished articles.
Physical Properties Metric English Comments
Mooney Viscosity 45 - 55

@Temperature 100 °C
45 - 55

@Temperature 212 °F
ML 1-4
Ash <= 0.20 %
<= 0.20 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
Tensile Strength, Yield >= 9.00 MPa
>= 1310 psi
Elongation at Break >= 360 %
>= 360 %
Chemical Properties Metric English Comments
Styrene Content 23 - 27 %
23 - 27 %
Descriptive Properties Value Comments
Loss During Drying <0.5%
Mass Share of Micro-Block Styrene <2%
Mass Share of Oil 25-29%
Spread Flow Batch Error <±8 %