Sibur KF-Z Carbamide Formaldehyde Resin

Category Polymer , Thermoplastic
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur KF-Z Carbamide Formaldehyde Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
In binding materials for production of wood laminate, base of glues for wood materials, for impregnation of paper during production of synthetic veneer sheet, production of varnish, production of rods and forms in the metallurgical industry. Mixing of resin with water at 10-21°C in ratio of 2:1.
Physical Properties Metric English Comments
Viscosity Measurement 10 - 20

@Temperature 19.5 - 20.5 °C
10 - 20

@Temperature 67.1 - 68.9 °F
(L), in viscometer VM-246 with 6 mm nozzle diameter
15 - 35

@Temperature 19.5 - 20.5 °C
15 - 35

@Temperature 67.1 - 68.9 °F
(F), in viscometer VM-246 with 6 mm nozzle diameter
Processing Properties Metric English Comments
Gel Time 0.670 - 1.083 min
0.670 - 1.083 min
At 100°C
Descriptive Properties Value Comments
Concentration of Hydrogen Ions 7.5-8.7 pH
Mass Fraction of Dry Residue 65-69%
Mass Fraction of Free Formaldehyde <0.9%
Ultimate Strength <1.5 MPa
In cutting of glue layer of plywood after 24 hours in water