Sibur Nitrilast-33M Nitrile-Butadiene Rubber (NBR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur Nitrilast-33M Nitrile-Butadiene Rubber (NBR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BYLT M-50 DN 202. For production of oil-benzene resistant articles for the automobile, aviation and rubber technical industries. Rubbers on the base of Nitrilast possess good oil-benzene resistance. Rubber mixtures on the base of Nitrilast are more resistant to wearing than those made of natural rubber.
Physical Properties Metric English Comments
Mooney Viscosity 43 - 68

@Temperature 100 °C
43 - 68

@Temperature 212 °F
ML 1-4
Ash <= 0.60 %
<= 0.60 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 23.5 MPa
>= 3410 psi
Elongation at Break >= 450 %
>= 450 %
Descriptive Properties Value Comments
Loss During Drying 0.007
Mass Share Adigol-2 0.5-1.2%
Mass Share of VS-30A 1-1.5%