Silberline EX 2871 Stabilized UV

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline EX 2871 Stabilized UV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EX 2871 provides a non-leafing, fine particle size grade of aluminum flake pigment for use in one pack UV cured coatings. The aluminum flake is stabilized to increase the shelf life of the product in such systems. A high concentration of metal flake in a non-reactive C13-15 fatty alcohol carrier ensures both maximum formulating flexibility and good system compatibility.Applications: Printing Inks
Physical Properties Metric English Comments
Specific Gravity 1.71 g/cc
1.71 g/cc
Volatiles 1.5 %
1.5 %
Particle Size 13 µm
13 µm
Before Conversion
Descriptive Properties Value Comments
% Carrier 25
Carrier Aliphatic Alcohol
Category Non-leafing