Silberline Sparkle Silvex® 760-20-D

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silvex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silvex® 760-20-D.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use in liquid colorant applications where processing temperatures are below the volatilization point of the carrier. Sparkle Silvex® D grades are compatible with a variety of resins including vinyl, polyolefins and styrene. Sparkle Silvex® D grades are dampened with diisodecyl phthalate. Sparkle Silvex® D grades can be used in vinyl screen printing ink formulations with good results. In order to maintain optimum aesthetics, Sparkle Silvex® grades should be dispersed properly.Applications: Plastics
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
Particle Size 55 µm
55 µm
Thermal Properties Metric English Comments
Flash Point 224 °C
435 °F
Descriptive Properties Value Comments
% Carrier 20
Carrier Diisodecylphthalate