Silikony Polskie Polsil OM 10 Methyl Silicone Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Silikony Polskie
Trade Name Polsil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silikony Polskie Polsil OM 10 Methyl Silicone Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gives the silicone fluids special usage properties. A surface covered with methyl silicone fluids reflects anti-adhesive properties, while the thin layer of oil remaining on it, is resistant to high temperature. Fluids may be sprayed both in the form of several-percent solution and non-diluted. In rubber processing also water emulsion of silicone fluids are used (Polsil® E), which are easy to dilute and apply.A surface covered with methyl silicone fluids reflects anti-adhesive properties, while the thin layer of oil remaining on it, is resistant to high temperature. Fluids may be sprayed both in the form of several-percent solution and non-diluted. In rubber processing also water emulsion of silicone fluids are used (Polsil® E), which are easy to dilute and apply.
Physical Properties Metric English Comments
Viscosity 10 cP

@Temperature 25.0 °C
10 cP

@Temperature 77.0 °F
Storage Temperature <= 40.0 °C
<= 104 °F