Sinotek Materials Graphite Felt Heat Insulation Material

Category Carbon , Graphite
Manufacturer Sinotek Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sinotek Materials Graphite Felt Heat Insulation Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sinotek
Physical Properties Metric English Comments
Bulk Density 0.120 g/cc
0.00434 lb/in³
Thickness <= 20000 microns
<= 787 mil
Ash <= 0.050 %
<= 0.050 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.450 W/m-K

@Temperature 1400 °C
3.12 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Component Elements Properties Metric English Comments
Carbon, C 98 %
98 %