Material Notes:
Chemical Name: COMPLEX CARBOHYDRATE POLYMER Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: AG-RHO® DR-2000 is a powdered form of HP guar for use as a drift reduction agent.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Viscosity >= 3000 cP
>= 3000 cP
1% in Water After 60 min; RP-0945
Processing Properties Metric English Comments
Moisture Content 3.5 - 9.0 %
3.5 - 9.0 %
RP-0838
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Pass, Per Standard
Dry, NGA-DA11
Dispersion Passes
No Lumps After 30sec, NGA DP16
Dry Flow Passes
NGA DF1