Solvay ALKAMULS® SC 242 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® SC 242 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 13.Identification: GLYCERYL POLYETHYLENEGLYCOL RICINOLEATECAS: 61791 – 12 – 6CEE ADDITIVE N° E 484Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifier, solubilizing agent.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 3.00 °C
37.4 °F
Flash Point >= 100 °C
>= 212 °F
Chemical Properties Metric English Comments
Total Acid Number <= 2.0
<= 2.0
[mg KOH/g]; RPG03
Processing Properties Metric English Comments
Moisture Content <= 3.0 %
<= 3.0 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous Liquid
Composition 1,4-Dioxane
<10 ppm
Active
0.97
HLB number 12.6
Hydroxyl Number 65-78 mg KOH/g
RPG06
Ionic Charge Nonionic
Saponification number 65-70 mg KOH/g
RPG05