Solvay ALKAMULS® T/20 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® T/20 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polysorbate 20 Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant fortextile industry. Nonionic sorbitan ester ethoxylate with an HLB of approx. 16.7. Useful as emulsifier for aliphatic oils and as a biological activator in adjuvants.Identification: ETHOXYLATED SORBITAN MONOLAURATECAS: 9005 – 64 – 5Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Agrochemical formulations: Useful as emulsifier for aliphatic oils and as a biologicalactivator in adjuvants. Industrial formulations: Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant for textile industry. Metal treatment: Sorbitan ester ethoxylate with a HLB of 16.7. Oil in water emulsifier for mineral and vegetable oils in metalworking. Solubilizer, antistat and lubricant for textile industry. Polymer systems specialities : Ethoxylated emulsifier and dispersant.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Chemical Properties Metric English Comments
Total Acid Number <= 2.0
<= 2.0
[mg KOH/g]; RPG03
Processing Properties Metric English Comments
Moisture Content <= 3.0 %
<= 3.0 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Liquid
Composition Active
0.97
HLB number 16.7
Hydroxyl Number 95-115 mg KOH/g
RPG06
Ionic Charge Nonionic
Saponification number 40-50 mg KOH/g
RPG05