Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay ALKAMULS® VO/2003 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® VO/2003 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: MIXTURE OF FATTY ACID POLYETHYLENE GLYCOL ESTERSCAS: 220037 – 02 – 5Solubility: Dispersible in water, soluble in most polar and aromatic solventsAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Agrochemicals formulations : Surfactant of choice for Oil based formulation. Excellent emulsifier for vegetable oils. Excellent dispersing properties. Specifically designed for OD formulation. Metal treatment : Nonionic emulsifier for vegetable oilsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
pH 7.0 - 8.0
7.0 - 8.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
RPG18
Chemical Properties Metric English Comments
Total Acid Number 10 - 14
10 - 14
[mg KOH/g]; RPG03
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear yellow liquid
RPG31
Composition Active
1
Ionic Charge Nonionic
Users viewing this material also viewed the following: