Solvay ANTAROX® BL 214 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ANTAROX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ANTAROX® BL 214 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: ETHOXYLATED PROPOXYLATED C8-C10 ALCOHOLSCAS: 68603-25-8; 7732-18-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX© BL-214 functions as a good foam control surfactant with excellent rewetting properties at temperatures as low as 25° C. ANTAROX© BL-214 is soluble in water and polar solvents. ANTAROX© BL-214 is used in ambient temperature spray metal cleaners, polyacrylamide emulsions, and textile finishing operations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
RP-0138
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to Slightly Hazy, Free Flowing Liquid
RP-0064
Cloud Point 12-16°C
1% Solution, RP-0124
Neutralization Number <0.5 mg KOH/mg
pH 7, RP-0343