Solvay ANTAROX® LAEP 15 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ANTAROX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ANTAROX® LAEP 15 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Branched alcohol EO/PO. Excellent hard surface cleaning with controlled foam. Very free rinsing. Also used in vehicle cleaners.Chemical Name: DETERGENT RANGE ALCOHOL ALKOXYLATECAS: 37251-67-5; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX© LAEP-15 is a branched alcohol EO/PO. It is excellent for hard surface cleaning with controlled foam. Very free rinsing. Also used in vehicle cleaners. Automatic-Dish Washing Detergents, Hard Surface Cleaners, Miscellaneous CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 6.0 - 8.0
6.0 - 8.0
5% Solution; RP-0420
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clean, Clear Liquid
RP-0064
Cloud Point 25-30°C
1.0% Solution, RP-0124