Material Notes:
Description: EO.PO block polymer. Multipurpose dispersing agent for suspension concentrate.Chemical Name: ETHYLENE/PROPYLENE OXIDE BLOCK POLYMERSolubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifier, dispersing agent.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 18.0 °C
64.4 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Composition Active
0.5
Ionic Charge Nonionic