Solvay Chemicals Ammonium Fluoride Grade 2 Aqueous solution of ammonium fluoride 40%

Category Fluid
Manufacturer Solvay Chemicals
Trade Name Ammonium Fluoride
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Ammonium Fluoride Grade 2 Aqueous solution of ammonium fluoride 40%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electronic Grade Ammonium Fluoride Ammonium fluoride: CAS-No.: 12125-01-8 / EC-No.: 235-185-9 / Index-No.: 009-006-00-8Uses: Etching agent and Electronic industryInformation provided by Solvay
Physical Properties Metric English Comments
Molecular Weight 37 g/mol
37 g/mol
Thermal Properties Metric English Comments
Melting Point 0.000 °C
32.0 °F
Boiling Point >= 100 °C
>= 212 °F
Descriptive Properties Value Comments
Appearance liquid
Color Colorless
Composition 0.4
Ammonium fluoride