Solvay Chemicals NOCOLOK® Sil Flux (extra fine grade)

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name NOCOLOK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals NOCOLOK® Sil Flux (extra fine grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reactive flux for brazing of aluminum and filler alloy generating flux for brazing aluminum Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Composition: either 2:1: 66.6 % ± 1.5 % -NOCOLOK Flux and 33.3 % ± 1.5 % -Silicon powder or 3:1: 75% ± 1.5 % -NOCOLOK Flux and 25% ± 1.5 % -Silicon powderUses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided by Solvay
Physical Properties Metric English Comments
Solubility in Water 0.45 %
0.45 %
NOCOLOK Flux
Thermal Properties Metric English Comments
Melting Point 564 - 572 °C
1050 - 1060 °F
NOCOLOK Flux
Descriptive Properties Value Comments
Appearance grey powder