Solvay Chemicals SOLKANE® 407C

Category Fluid
Manufacturer Solvay Chemicals
Trade Name SOLKANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals SOLKANE® 407C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HFC SOLKANE® 407C replaces R22 in air conditioning systems and water chillers for temperature ranges from -40°C up to 10°C. Pentafluoroethane- CAS-No.: 354-33-6 / EC-No.: 206-557-8 / REACH Registration Number: 01-2119485636-25 and 1,1,1,2 Tetrafluoroethane- CAS-No.: 811-97-2 / EC-No.: 212-377-0 / REACH Registration Number: 01-2119459374-33 and Difluoromethane- CAS-No.: 75-10-5 / EC-No.: 200-839-4 Uses: RefrigerantInformation provided by Solvay
Thermal Properties Metric English Comments
Melting Point -103 °C
-153 °F
Pentafluoroethane
Boiling Point -44.0 - -37.0 °C
-47.2 - -34.6 °F
Descriptive Properties Value Comments
Appearance compressed liquefied gas
Color colorless
Composition 0.23
Difluoromethane
0.25
Pentafluoroethane
0.52
1,1,1,2 Tetrafluoroethane