CAS Number: 127-18-4/EINECS: 204-825-9/UN: 1897Information provided by Solvay
Physical Properties Metric English Comments
Density 1.615 - 1.621 g/cc
0.05835 - 0.05856 lb/in³
D<sub>20/4</sub>
pH >= 8.0
>= 8.0
Molecular Weight 165.8 g/mol
165.8 g/mol
Descriptive Properties Value Comments
Appearance Clear without suspended matter
ASTM D3741/B
Color <15
APHA
Composition <1 mg/kg
Oxidizing Compounds (Cl2), ASTM D4755
<30 mg/kg
Alkalinity (NaOH), ASTM D2989
<30 mg/kg
Non volatile Reside, ASTM D1353
<30 mg/kg
Moisture (H2O), Karl Fischer, ASTM E1064
>1 mg/kg
Acid Acceptance (NaOH)
Purity >999 g/kg
without Stabilizers