Material Notes:
Strontium carbonate coarse powder is used in the production of glazes, frits and for production of strontium pigments. Another application for strontium carbonate coarse powder is the production of special glass.Information provided by Solvay
Physical Properties Metric English Comments
Bulk Density 1.00 - 1.60 g/cc
0.0361 - 0.0578 lb/in³
loose
Descriptive Properties Value Comments
Composition <0.5%
Sulfur as SO3
>98%
SrCO3/BaCO3 (HCI-Titration)
Sieve Analysis <1%
>2 nm
<5%
>0.063 nm