Solvay DERMALCARE® MAP L 210 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name DERMALCARE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay DERMALCARE® MAP L 210 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High purity Monoalkyl Phosphate based off patented Rhodia process. Upon neutralization, MAP L-210 is extremely mild to the skin and imparts a soft elegant skin feel. Provides a dense, creamy lather to formulated products.Chemical Name: COMPLEX ORGANIC PHOSPHATE ESTER, FREE ACIDCAS: 39464-66-9, 4536-30-5, 7664-38-2Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DERMALCARE MAP-L-210 is a high purity Laureth-1 Phosphate ester in the free acid form. Typically used in facial and skin cleanser applications, Dermalcare MAP-L 210 can be neutralized with any common base to yield ultra-mild surfactants that produce a luxurious, creamy lather. In formulated systems, Dermalcare MAP-L-210 imparts an elegant, soft feel to skin.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH <= 2.5
<= 2.5
10% Solution; RP-0402
Optical Properties Metric English Comments
Gardner Color Number <= 1.0

@Temperature 50.0 °C
<= 1.0

@Temperature 122 °F
RP-0138
Chemical Properties Metric English Comments
Total Acid Number 176 - 184
176 - 184
(100% Basis); RP-0427
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White to pale yellow, low MP soft solid
RP-0064
Composition Free Acid (As H3PO4)
<7%, RP-0427
Nonionics
<6%, RP-0966