Solvay GEROPON® DOS/PG Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name GEROPON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GEROPON® DOS/PG Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: SODIUM DIOCTYLSULPHOSUCCINATE IN GLYCOL WATER SOLUTIONCAS: 577 – 11 – 7; 57 – 55 – 6; 7732 – 18 – 5Solubility: Dispersible in water and polar solvents. Soluble in most aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Wetting agent, emulsifier, de-emulsifier. Used in specialty cleaners, dewatering agent for flotation concentrates, oil spill clean-up blends. High flash point compatibility agent for herbicide SE formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Limpid liquid
RPG31
Composition Active content
0.65
Dry substance
64-66%, RPG25
Ionic Charge Anionic