Material Notes:
Identification: Nonylphenol Ethoxylate (30 EO)CAS: 68412 – 54 – 4Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL CO-887 is a Nonionic co-emulsifier generally used for emulsion/polymerization.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 70 - 73 %
70 - 73 %
CEM, 60% Power; RP-0528
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
RP-0064
Cloud Point 74-78°C
1% in 10% Salt Sol., RP-0124
Color <100
APHA, RP-0134
Hydroxyl Number 36-40 mg KOH/g
Before water, RP-0245
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343