Solvay JAGUAR® C 500 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name JAGUAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay JAGUAR® C 500 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Light conditioning performance with enhanced volume and good wet compatibilityChemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: Guar Hydroxypropyltrimonium ChlorideCAS: 65497-29-2Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Jaguar C-500 is a cationic polymer derived from a natural gum with low aqueous viscosity. Jaguar C-500 is an excellent additive to aid in the deposition of actives such as silicones, oils, anti-dandruff agents on hair where viscosity build-up in the final product is not desired. Ideal application is one where deposition of actives from a shampoo or conditioner which requires little viscosifying properties. Easily and quickly dispersible in water. Recommended use levels: 0.1 – 2.0%.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Viscosity 25 - 65 cP
25 - 65 cP
V-264-0
Component Elements Properties Metric English Comments
Nitrogen, N 1.15 - 1.45 %
1.15 - 1.45 %
RP-885
Processing Properties Metric English Comments
Moisture Content 5.0 - 10 %
5.0 - 10 %
RP-1429
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Off white to light yellow powder
DA-20-0
Composition Gram Negative Bacteria
Negative, RP-1445
Molds and yeasts
<100 cfu/g, RP-1445
Plate Count
<500 cfu/g, RP-1410
Staphylococcus Aureus
Negative, RP-1445
Odor Low, characteristic