Solvay LUBRHOPHOS® LB 400 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name LUBRHOPHOS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay LUBRHOPHOS® LB 400 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: POLYOXYETHYLENE OCTADECENYL ETHER PHOSPHATECAS: 39464-69-2, 9004-98-2, 7664-38-2, 7664-38-2Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: LUBRHOPHOS LB-400 is a lubricant and anti-wear additive, corrosion inhibitor, wetting agent, emulsifier, detergent, dispersant for lubricating and rolling oils, hydraulic and water-based cutting fluids, glass cutting and polishing lubricants. Biodegradable and non ecotoxic surfactant.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Optical Properties Metric English Comments
Gardner Color Number <= 2.0
<= 2.0
RP-0138
Chemical Properties Metric English Comments
Total Acid Number 82 - 92
82 - 92
KOH to First Infl. PT.; RP-0427
Processing Properties Metric English Comments
Moisture Content <= 2.0 %
<= 2.0 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Viscous Opaque liquid
Separates on standing, RP-0064
Composition Nonionic content
<8.0%, RP-0351